Abstract
The ziziphus spina-Christi extract (ZSC) was applied as a corrosion inhibitor for aluminum alloy 7051 (A7051) in an acidic medium, 0.1 M HCl. The potentiodynamic polarization measurement was employed to investigate the inhibitor's corrosion inhibition efficiency at various concentrations and different temperatures. The results showed a high inhibition efficiency, up to 95.84% at 7 ppm concentration at a lower examined temperature, indicating effective adsorption of the inhibitor molecule at the aluminium alloy surface.
The polarization data revealed that ZSC acts as a mixed-type corrosion inhibitor be effecting both cathodic reaction ( hydrogen evolution) and anodic reaction (metal dissolution). The influence of temperature was examined through Arrhenius and transition state approaches, showing that an increase in activation energy (Ea) occurred after adding ZSC. Adsorption behavior was examined using the Langmuir adsorption isotherm, and the calculated standard free energy of adsorption values confirmed a spontaneous adsorption process dominated by physical interactions.
The inhibition mechanism was attributed to the formation of a protective adsorbed film involving electrostatic interactions and donor–acceptor bonding between ZSC constituents and the A7051 surface. These findings suggest that Ziziphus spina-Christi leaves extract is an effective and environmentally friendly corrosion inhibitor for A7051 in acidic environments.
Keywords
Corrosion, Corrosion inhibitor, Ziziphus spina-Christi, Aluminum alloy
Downloads
References
1. Kamil, F.H., et al., Corrosion Behaviour, Kinetic and Thermodynamic Studies of Water Hyacinth Extract as a Corrosion Inhibitor for Low-Carbon Steel. Iraqi Journal of Industrial Research, 2024. 11(3): p. 35-44. [Google Scholar] [Crossref]
2. Kadhim, A., et al., Corrosion inhibitors. A review. International Journal of Corrosion and Scale Inhibition, 2021. 10(1): p. 54-67. [Google Scholar] [Crossref]
3. Hossain, N., M. Asaduzzaman Chowdhury, and M. Kchaou, An overview of green corrosion inhibitors for sustainable and environment friendly industrial development. Journal of Adhesion Science and Technology, 2021. 35(7): p. 673-690. [Google Scholar] [Crossref]
4. Natarajan, R. and F.S.Z.S. Al Shibli, Synthesis of biomass derived product from Ziziphus spina-christi and application for surface protection of metal under acidic environment-Performance evaluation and thermodynamic studies. Chemosphere, 2021. 284: p. 131375. [Google Scholar] [Crossref]
5. Shahryari, Z. and K. Gheisari, Corrosion inhibition properties of Ziziphus spina-christi leaves extract and zinc cations on mild steel in sodium chloride solution. Materials Chemistry and Physics, 2023. 299: p. 127474. [Google Scholar] [Crossref]
6. Al-Ashoor, S.Z., D.S. Ali, and H.Z. Al-Sawaad, Ziziphus spina Christi leaves methanol extract evaluation as antifungal, antibacterial, antioxidant and green inhibitor for carbon steel alloy corrosion in hydrochloric acid. Portugaliae Electrochimica Acta, 2023. 41(2): p. 167-184. [Google Scholar] [Crossref]
7. Sargenti, S.R. and W. Vichnewski, Sonication and liquid chromatography as a rapid technique for extraction and fractionation of plant material. Phytochemical Analysis: An International Journal of Plant Chemical and Biochemical Techniques, 2000. 11(2): p. 69-73. [Google Scholar] [Crossref]
8. Yeasmen, N. and V. Orsat, Pulsed ultrasound assisted extraction of alternative plant protein from sugar maple leaves: Characterization of physical, structural, thermal, electrical, and techno-functional properties. Food Hydrocolloids, 2024. 152: p. 109960. [Google Scholar] [Crossref]
9. Al-Mashhadani, H.A., et al. Anti-corrosive substance as green inhibitor for carbon steel in saline and acidic media. in Journal of Physics: Conference Series. 2021. IOP Publishing. [Google Scholar] [Crossref]
10. Jehad, M.H., et al., Anodizing of pure aluminum alloy with incorporated ferric oxide nanoparticles to enhance the aluminum corrosion resistance. Research Journal of Pharmacy and Technology, 2023. 16(6): p. 2935-2940. [Google Scholar] [Crossref]
11. Alshujery, M.K. and K.A.S. Al-Saadie. Corrosion inhibition of aluminum 6061 alloy by a micro arc oxidation modified with incorporated zinc oxide nanoparticles. in 4TH INTERNATIONAL SCIENTIFIC CONFERENCE OF ENGINEERING SCIENCES AND ADVANCES TECHNOLOGIES. 2023. AIP Publishing LLC. [Google Scholar] [Crossref]
12. Mohammed, R. and H. Almashhadani, Synthesis, characterization and thermodynamic study of a polymer nanocomposite from methyl acrylate and zirconium chloride as an anti-corrosion coating for carbon steel. Int. J. Corros. Scale Inhib, 2023. 12(3): p. 1180-1191. [Google Scholar] [Crossref]
13. Vera, J., K. Evans, and C. Mendez. Derivation of a Modified Stern-Geary Linear Polarization Equation. Application to seawater corrosion and inhibitor evaluation. in CONFERENCE 2024. 2024. Association for Materials Protection and Performance. [Google Scholar] [Crossref]
14. Koga, N., A review of the mutual dependence of Arrhenius parameters evaluated by the thermoanalytical study of solid-state reactions: the kinetic compensation effect. Thermochimica acta, 1994. 244: p. 1-20. [Google Scholar] [Crossref]
15. Mahmmod, A.A., et al., Quinoxaline as a corrosion inhibitor for copper in nitric acid: Kinetics, statistical, and theoretical investigations. Case Studies in Chemical and Environmental Engineering, 2024. 10: p. 100836. [Google Scholar] [Crossref]
16. de Lima, A.C.A., et al., Adsorption Thermodynamics, in Adsorption. CRC Press. p. 76-110. [Google Scholar] [Crossref]
17. Nandee, R., et al., Surface topography and surface morphology of graphene nanocomposite by FESEM, EDX and AFM analysis. Nano-Structures & Nano-Objects, 2024. 38: p. 101170. [Google Scholar] [Crossref]
18. Kairi, N.I. and J. Kassim, The effect of temperature on the corrosion inhibition of mild steel in 1 M HCl solution by Curcuma longa extract. International Journal of Electrochemical Science, 2013. 8(5): p. 7138-7155. [Google Scholar] [Crossref]
19. Alshujerya, M.K. and K.A.S. Al-Saadiea, Aluminum 6061 Alloy Modification with Micro Arc Oxidation and Ferric Oxide Nanoparticles Incorporated to Reduce Aluminum Corrosion. Egyptian Journal of Chemistry, 2023. 66(5): p. 99-105. [Google Scholar] [Crossref]
20. Holla, B.R., et al., Plant extracts as green corrosion inhibitors for different kinds of steel: A review. Heliyon, 2024. 10(14). [Google Scholar] [Crossref]
21. Shathani, P., et al., Plant leaves extracts as green corrosion inhibitors of steel in acidic and seawater environments: a review. Environmental Science and Pollution Research, 2025: p. 1-22. [Google Scholar] [Crossref]
Metrics
Views & Downloads
Similar Articles
- Green Synthesis of Cobalt Oxide/Gold (Coo/Au) Bimetallic Nanoparticles Using Sinapinic Acid: A Comprehensive Study
- Advances in Solar Cell Technologies: A Comprehensive Review of Material Synthesis, Structural Properties, Efficiency and Diverse Applications
- Thermal Decomposition of Co-Fe-Cr-Citrate Complex Via Structural and Spectral Study
- Surface Activity and Thermodynamic Assessment of Surfactants Derived from Oreochromis Niloticus Oil (Nile Tilapia Fish)
- Green Synthesis of Robust Metal-Organic Frameworks: A Sustainable Approach for Advanced Applications